Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 39.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 39.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 39.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Europe-Africa-Middle East) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |