Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 38.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 38.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 38.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Asia Pacific) LNP LUBRICOMP* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 38.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Asia Pacific) LNP LUBRICOMP* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |