Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 67.5 µm/m-°C

@Temperature -40.0 - 95.0 °C
37.5 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
CTE, linear, Parallel to Flow 67.5 µm/m-°C

@Temperature 23.0 - 80.0 °C
37.5 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
CTE, linear, Parallel to Flow 67.5 µm/m-°C

@Temperature -40.0 - 95.0 °C
37.5 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
CTE, linear, Parallel to Flow 67.5 µm/m-°C

@Temperature 23.0 - 80.0 °C
37.5 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
CTE, linear, Parallel to Flow 67.5 µm/m-°C

@Temperature -40.0 - 95.0 °C
37.5 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by ..
CTE, linear, Parallel to Flow 67.5 µm/m-°C

@Temperature 23.0 - 80.0 °C
37.5 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by ..