Polymer Property : CTE, linear, Parallel to Flow = 36.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 65.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 65.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 65.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC (Asia Pacific)
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 65.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC (Asia Pacific)
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.