Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 32.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF008ER PC LNP THERMOCOMP* DF008ER is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Easy Molding, Mold Release. |
|||
CTE, linear, Parallel to Flow | 32.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF008ERH PC LNP THERMOCOMP* DF008ERH is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |