Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.4 µm/m-°C

@Temperature 23.0 - 150 °C
16.9 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East)
VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles.
CTE, linear, Parallel to Flow 30.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific)
LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber.
CTE, linear, Parallel to Flow 30.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF006H PA 66
LNP THERMOCOMP* RF006H is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare.
CTE, linear, Parallel to Flow 30.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RF006H PA 66
LNP THERMOCOMP* RF006H is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare.
CTE, linear, Parallel to Flow 30.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF006XXZ PA 66
LNP THERMOCOMP* RF006XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber
CTE, linear, Parallel to Flow 30.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RF006XXZ PA 66
LNP THERMOCOMP* RF006XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber
CTE, linear, Parallel to Flow 30.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11
LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber.