Polymer Property : CTE, linear, Parallel to Flow = 3.17 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 5.70 µm/m-°C

@Temperature -40.0 - 40.0 °C
3.17 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East)
High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 5.70 µm/m-°C

@Temperature -40.0 - 40.0 °C
3.17 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East)
High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.