Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 5.50 µm/m-°C @Temperature <=143 °C |
3.06 µin/in-°F @Temperature <=289 °F |
Below Tg; ISO 11359 |