Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 46.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East)
VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.