Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 25.3 µm/m-°C @Temperature -30.0 - 80.0 °C |
14.1 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 non-halogen FR compound |