CTE, linear, Parallel to Flow 200 µm/m-°C

@Temperature 23.0 - 55.0 °C
111 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6  (Unverified Data**)
Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene..
CTE, linear, Parallel to Flow 200 µm/m-°C

@Temperature 23.0 - 55.0 °C
111 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6  (Unverified Data**)
Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene..