Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 20.5 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 20.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |