Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 190 µm/m-°C

@Temperature 150 - 250 °C
106 µin/in-°F

@Temperature 302 - 482 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in water-c..
CTE, linear, Parallel to Flow 190 µm/m-°C

@Temperature -30.0 - 90.0 °C
106 µin/in-°F

@Temperature -22.0 - 194 °F
3
Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE)
Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r..
CTE, linear, Parallel to Flow 190 µm/m-°C

@Temperature 23.0 - 150 °C
106 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors