Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 35.7 µm/m-°C

@Temperature 23.0 - 150 °C
19.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East)
10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.