Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 126 µm/m-°C @Temperature 23.0 - 55.0 °C |
70.0 µin/in-°F @Temperature 73.4 - 131 °F |
|
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
CTE, linear, Parallel to Flow | 126 µm/m-°C @Temperature 25.6 - 93.3 °C |
70.0 µin/in-°F @Temperature 78.0 - 200 °F |
Length |
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
CTE, linear, Parallel to Flow | 126 µm/m-°C @Temperature 25.6 - 149 °C |
70.0 µin/in-°F @Temperature 78.0 - 300 °F |
Length |
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
CTE, linear, Parallel to Flow | 126 µm/m-°C @Temperature 60.0 - 138 °C |
70.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
CTE, linear, Parallel to Flow | 126 µm/m-°C @Temperature 60.0 - 138 °C |
70.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific) Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
CTE, linear, Parallel to Flow | 126 µm/m-°C @Temperature 23.0 - 55.0 °C |
70.0 µin/in-°F @Temperature 73.4 - 131 °F |
|
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |