Polymer Property : CTE, linear, Parallel to Flow = 124 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature 60.0 - 138 °C
68.9 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 357 PBT
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature 60.0 - 138 °C
68.9 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific)
PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature 60.0 - 138 °C
68.9 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 357 PBT+PC
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature 60.0 - 138 °C
68.9 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature 60.0 - 138 °C
68.9 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 357U PBT
Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature 60.0 - 138 °C
68.9 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific)
Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature 60.0 - 138 °C
68.9 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 357U PBT+PC
Unreinforced PC/PBT, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature -40.0 - 40.0 °C
68.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal
LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature -40.0 - 40.0 °C
68.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal
LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature -40.0 - 40.0 °C
68.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT
LNP* STAT-LOY* WF306C is a compound based on PBT resin containing 30% Glass Fiber. Added features of this material include: Antistat, Clean Compound System.
CTE, linear, Parallel to Flow 124 µm/m-°C

@Temperature -40.0 - 40.0 °C
68.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific)
LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System.