Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 21.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features include: Exceptional Processing, Non-Brominated & Non-Chlorinated Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 21.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC (Asia Pacific) LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing, Flame Retardant, Non-Br.. |