Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 107 µm/m-°C

@Temperature -40.0 - 40.0 °C
59.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly
LNP* THERMOCOMP* KFB11 is a compound based on Acetal Copolymer resin containing 5% Glass Fiber, 5% Glass Bead. Added features of this material include: Low Warpage, Chemically Coupled.
CTE, linear, Parallel to Flow 107 µm/m-°C

@Temperature -40.0 - 40.0 °C
59.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KFB11 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled.