Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 1.02 µm/m-°C

@Temperature 23.0 - 60.0 °C
0.567 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched
LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding
CTE, linear, Parallel to Flow 1.02 µm/m-°C

@Temperature -40.0 - 40.0 °C
0.567 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched
LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding
CTE, linear, Parallel to Flow 1.02 µm/m-°C

@Temperature 23.0 - 60.0 °C
0.567 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched
LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding
CTE, linear, Parallel to Flow 1.02 µm/m-°C

@Temperature -40.0 - 40.0 °C
0.567 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched
LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding