Polymer Property : Hot Ball Pressure Test = 85.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Hot Ball Pressure Test 75.0 - 85.0 °C
167 - 185 °F
Average value: 80.8 °C Grade Count:12
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..