Polymer Property : Hot Ball Pressure Test = 428 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Hot Ball Pressure Test 220 °C
428 °F
BS 3456, IEC 335
EPICHEM Epinyl PA 66 GF25 AU Polyamide 66, 25% Glass, Self extinguishing
Characteristics: 25% glass fibre filled
Hot Ball Pressure Test 220 °C

@Thickness 3.00 mm
428 °F

@Thickness 0.118 in
IEC 60695-10-2
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded
Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym..