Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | 82.0 °C | 180 °F | IEC335-1 |
Supreme Petrochem SP 515 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any colorProcessing Injection molding Extrusion Applications Electrical switch boards MCB distribution bo.. |
|||
Hot Ball Pressure Test | 82.0 °C | 180 °F | IEC335-1 |
Supreme Petrochem SP 553 Flame Retardant Polystyrene Characteristics High flow properties Good balance of toughness and rigidity Available in any color Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxes, electric.. |
|||
Hot Ball Pressure Test | 82.0 °C | 180 °F | IEC335-1 |
Supreme Petrochem SP 556 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any color Processing Extrusion MoldingApplications T.V. Cabinets, computer monitor, printer housing Elect.. |