Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | 138 °C | 280 °F | IEC 60695-10-2 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Hot Ball Pressure Test | 138 °C | 280 °F | IEC 60695-10-2 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Hot Ball Pressure Test | 138 °C | 280 °F | IEC 60695-10-2 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Hot Ball Pressure Test | 138 °C | 280 °F | IEC 60695-10-2 |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Hot Ball Pressure Test | 138 °C | 280 °F | IEC 60695-10-2 |
Covestro Makrolon® 3158 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Hot Ball Pressure Test | 138 °C | 280 °F | IEC 60695-10-2 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Hot Ball Pressure Test | 138 °C | 280 °F | IEC 60695-10-2 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |