Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | >= 128 °C | >= 262 °F | BS 3456, IEC 335 |
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact Characteristics: high fluidity, high impact |
|||
Hot Ball Pressure Test | >= 128 °C | >= 262 °F | BS 3456, IEC 335 |
EPICHEM Epicarb PC Polycarbonate Characteristics: high fluidity, good impact |