Polymer Property : Liquidus = 890.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 890.6 °C
1635 °F
Flow Point
Lucas-Milhaupt Lithobraze 925 Silver Based Cadmium Free Filler Metal
Applications: The principal use to date of Litho braze 925 has been the brazing of honeycomb panel sections. It can be used for general purpose furnace brazing of stainless steels where flux must ..
Liquidus 890.6 °C
1635 °F
Universal Wire Works BAg-19 (AMS 4767) Silver Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.