Polymer Property : Liquidus = 72.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 72.0 °C
162 °F
Indium Corp. Indalloy® 162 In-Bi Fusible Alloy
Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation.