Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 350 °C | 662 °F | |
Johnson Matthey JM A-Core Soft Solder Flux The standard "acid" flux core used for most industrial applications where an aggressive flux is required. Residues are corrosive.Information provided by Johnson Matthey. |
|||
Liquidus | 350 °C | 662 °F | |
Johnson Matthey JM No1S Soft Solder Flux A highly active liquid flux recommended for use on Stainless and carbon steels. Generally used with the Silver/Tin alloys such as JM P40 and JM P5. Residues are corrosive and should be removed aft.. |