Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 245 °C | 473 °F | Flow Point |
Lucas-Milhaupt Clean & Bright 5 Tin/ Silver Solder Characteristics:This alloy is considered to be high strength solders. It has much higher creep strengths than the tin/lead solders. It is a good color match for stainless steel, and used with the p.. |