Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 452 °C | 845 °F | Flow Point |
Lucas-Milhaupt AL 815 Aluminum Brazing Filler Metal Characteristics:AL 815 is a general purpose free flowing soldering filler metals for use with all solderable aluminum and aluminum alloys when soldering with torch. Information provided by Lucas-Mi.. |