Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 233 °C | 451 °F | |
Indium Corp. Indalloy® 209 Sn-Ag-Sb Solder Alloy Low temperature die attach alloy. Has very high tensile strength. Old Motorola die attach solder; very brittle.Information provided by the manufacturer, Indium Corporation. |