Polymer Property : Liquidus = 424 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 218 °C
424 °F
Indium Corp. Indalloy 120 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Liquidus 218 °C
424 °F
AIM 95Sn/3.5Ag/1.5In Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Liquidus 218 °C
424 °F
AIM SAC305 Lead-Free Solder for Photonic Packaging
This alloy falls under the JEIDA recommendation for lead-free soldering. When used in wave soldering, AIM’s SAC305 bar solder offers far superior fluidity as compared to other alloys and makes of b..