Thermal Properties Metric English Comments
Liquidus 320 °C
608 °F
Indium Corp. Indalloy 168 Lead Solder Alloy
Information Provided by Indium Corporation
Liquidus 320 °C
608 °F
Johnson Matthey LM 15 Soft Solder/Flux
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi..