Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 299 °C | 570 °F | |
Indium Corp. Indalloy® 228 Pb-Sn-Ag Solder Alloy (Sn10) High temp solder. Not recommended for applications above 120°C, due to formation of eutectic.Information provided by the manufacturer, Indium Corporation. |
|||
Liquidus | 299 °C | 570 °F | |
Johnson Matthey JM1090 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |