Polymer Property : Liquidus = 2770 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 1520 °C
2770 °F
Johnson Matthey HS Platinum Jewelry Alloy
Hard springy, can be cast for catches.