Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1450 °C | 2640 °F | |
Goodfellow Iron 50/Nickel 50 Alloy Information provided by Goodfellow. |
|||
Liquidus | 1450 °C | 2640 °F | |
Goodfellow Iron 55/Nickel 45 Alloy Low Nickel magnetic alloy. Most applications are based on the requirements of moderately high saturation and permeabilities greater than silicon irons. Uses include the manufacture of sensitive rela.. |
|||
Liquidus | 1450 °C | 2640 °F | Melting Point |
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy) Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif.. |