Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1375 °C | 2507 °F | |
Special Metals NIMONIC® Alloy 81 A precipitation-hardenable nickel-chromium alloy with enhanced resistance to high-temperature corrosion. The excellent hot-corrosion resistance of the alloy results from its high chromium content o.. |