Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 225 °C | 437 °F | |
Indium Corp. Indalloy 251 Tin Solder Alloy Castin Patented alloyInformation Provided by Indium Corporation |
|||
Liquidus | 225 °C | 437 °F | |
Johnson Matthey Plumbsol Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Liquidus | 225 °C | 437 °F | |
Lucas-Milhaupt Silvabrite® Lead-Free Solder Silvabrite silver/tin soldering alloys have been engineered specifically for field repair. These silver/tin solders have been specifically formulated to make difficult repairs swiftly and confidentl.. |
|||
Liquidus | 225 °C | 437 °F | |
Williams Advanced Alloys WS225 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Liquidus | 225 °C | 437 °F | |
AIM 40In/60Pb Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |