Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1000 °C | 1830 °F | |
Osprey Metals HTN 2 Brazing Powder Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme.. |
|||
Liquidus | 1000 °C | 1830 °F | |
Williams Advanced Alloys Wambraze™ WB1000 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |