Polymer Property : Liquidus = 1680 °F
Polymer Property :
Liquidus =
1680 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Liquidus
915
°C
1680
°F
Wieland 1914 Wilaform Gold
Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental