Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 74.0 °C | 165 °F | Flow Point |
Aremco Crystalbond™ 509 Washaway Mounting Adhesive & Accessory Provides excellent adhesion and minimizes clogging of diamond tools compared to waxes. Transparent in thin cross-sections. Soluble in acetone or 509-S stripper, an odorless, non-flammable, biodegrad.. |