Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 807.2 °C | 1485 °F | |
Lucas-Milhaupt Silvaloy® 6 Brazing Alloy Silvaloy 6 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It should not be used on ferrous and nickel metals or copper.. |