Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Liquidus = 1450 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 785 °C
1450 °F
Johnson Matthey Matti-phos 2 Alloy for Fluxless Brazing of Copper
This alloy is less expensive than other Matti-phos alloys. It has good flow and ductility, and has the same uses as Copper-flo.Optimum Joint Gap 0.05 - 0.2 mm.AWS A5.8-92 BCuP-6BS EN 1044 1999 CP10..
Liquidus 785 °C
1450 °F
Indium Corp. Indalloy 220 Silver Solder Alloy
Information Provided by Indium Corporation
Liquidus 788 °C
1450 °F
Flow Point
Lucas-Milhaupt BRAZE 750 (Hard) Silver Based Cadmium Free Filler Metal
Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel..
Liquidus 788 °C
1450 °F
Lucas-Milhaupt Silvaloy® 2 Brazing Alloy
Silvaloy 2 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on ..