Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 779.4 °C | 1435 °F | Flow Point |
Lucas-Milhaupt BRAZE 403 Carbide Brazing Alloy Applications: Braze 403 is a good intermediate temperature brazing alloy for use on stainless steels, mild steels, cast and malleable irons and various nonferrous alloys. This alloy is particularly.. |
|||
Liquidus | 779.4 °C | 1435 °F | Flow Point |
Lucas-Milhaupt BRAZE 720 Silver Based Cadmium Free Filler Metal Characteristics:Brazing 720 is the silver-copper eutectic composition and in melting it acts like a metallic element, i.e. it melts completely at a single temperature, thus it will quickly flow into.. |
|||
Liquidus | 779.4 °C | 1435 °F | Flow Point |
Lucas-Milhaupt BRAZE 721 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc.. |
|||
Liquidus | 779.4 °C | 1435 °F | Flow Point |
Lucas-Milhaupt BRAZE 721 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc.. |
|||
Liquidus | 779.4 °C | 1435 °F | Flow Point |
Lucas-Milhaupt Lucanex 721 Active Metal Brazing Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste |
|||
Liquidus | 779.4 °C | 1435 °F | Flow Point |
Lucas-Milhaupt SIL-FOS 2 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 2 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi.. |
|||
Liquidus | 779.4 °C | 1435 °F | |
Lucas-Milhaupt Silvaloy® B72 Brazing Alloy Silvaloy B72 is the eutectic composition of the silver-copper system. It is suitable for use in controlled atmosphere brazing without the use of a paste flux. When molten, it is very fluid and may f.. |
|||
Liquidus | 779.4 °C | 1435 °F | Flow Point |
Lucas-Milhaupt Cerametil 721 Active Metal Brazing BR 721 strip coated for joining ceramics without metallization.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal strip in wrought Cerametil |