Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 136 °C | 277 °F | |
Indium Corp. Indalloy 76 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 136 °C | 277 °F | |
Indium Corp. Indalloy 78 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 136 °C | 277 °F | |
Indium Corp. Indalloy 79 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |