Polymer Property : Liquidus = 1190 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 643 °C
1190 °F
Flow Point
Lucas-Milhaupt SIL-FOS 18 Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos 18 is a moderate cost brazing filler metal suitable for joining copper, brass and bronze alloys where low brazing temperature and free flowing characteristics are required. I..