Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 585.0 °C | 1085 °F | Flow Point |
Lucas-Milhaupt AL 716 Aluminum Brazing Filler Metal Applications:AL 716 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought.. |