Polymer Property : Liquidus = 1082 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 1082 °C
1980 °F
Materion Brush 1915â„¢ Annealed Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Liquidus 1082 °C
1980 °F
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Liquidus 1082 °C
1980 °F
Materion Brush 1915â„¢ AT Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Liquidus 1082 °C
1980 °F
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Liquidus 1082 °C
1980 °F
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Liquidus 1082 °C
1980 °F
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Liquidus 1082 °C
1980 °F
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are..