Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 988 °C | 1810 °F | |
Wall Colmonoy COLMONOY® 88 Hard-Surfacing Alloy Description: Colmonoy 88 is a unique alloy containing fine, multiple hard phases which are uniformly distributed throughout a Ni-Cr-B matrix. These hard phases, comprised of complex bi- and tri-met.. |