Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 98.0 °C | 208 °F | |
Indium Corp. Indalloy 48 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 98.0 °C | 208 °F | |
Indium Corp. Indalloy 54 Bismuth Solder Alloy Information Provided by Indium Corporation |