Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 949 °C | 1740 °F | |
Universal Wire Works BNi-1A (AMS 4776) Nickel Base Brazing Filler Metal Low Carbon (compare to BNi-1)Information provided by Universal Wire Works for their line of welding wire and filler metal. |